dc.description.abstractSteels T23 and T24 developed as materials for welding water cooling membranes without using post-welding heat treatment are studied. The mechanical properties and the microstructure of welds of these steels are determined in the initial condition and after tempering. It is shown that post-welding treatment of welds of steels T23 and T24 is a necessary operation.cs
dc.format.extent1000691 bytescs
dc.format.mimetypeapplication/pdfcs
dc.language.isoencs
dc.publisherSpringercs
dc.relation.ispartofseriesMetal science and heat treatmentcs
dc.relation.urihttp://dx.doi.org/10.1007/s11041-011-9401-3cs
dc.subjectthermal power plantscs
dc.subjectweldscs
dc.subjectchromium-nickel steelscs
dc.titleEffect of post-welding heat treatment on secondary hardening of welded joints of Cr – Mo – V steelcs
dc.typearticlecs
dc.identifier.locationNení ve fondu ÚKcs
dc.identifier.doi10.1007/s11041-011-9401-3
dc.rights.accessopenAccess
dc.type.versionsubmittedVersion
dc.type.statusPeer-reviewedcs
dc.description.sourceWeb of Sciencecs
dc.description.volume53cs
dc.description.issue7-8cs
dc.description.lastpage378cs
dc.description.firstpage374cs
dc.identifier.wos000298330100014


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record