dc.contributor.author | Valiev, Ruslan Z. | |
dc.contributor.author | Semenova, Irina P. | |
dc.contributor.author | Latysh, Vladimir V. | |
dc.contributor.author | Rack, Henry | |
dc.contributor.author | Lowe, Terry C. | |
dc.contributor.author | Petruželka, Jiří | |
dc.contributor.author | Dluhoš, Luděk | |
dc.contributor.author | Hrušák, Daniel | |
dc.contributor.author | Sochová, Jarmila | |
dc.date.accessioned | 2008-10-13T13:17:48Z | |
dc.date.available | 2008-10-13T13:17:48Z | |
dc.date.issued | 2008 | |
dc.identifier.citation | Advanced engineering materials. 2008, vol. 10, issue 8, p. B15-B17. | en |
dc.identifier.issn | 1438-1656 | |
dc.identifier.issn | 1527-2648 | |
dc.identifier.uri | http://hdl.handle.net/10084/68093 | |
dc.language.iso | en | en |
dc.publisher | Wiley-VCH | en |
dc.relation.ispartofseries | Advanced Engineering Materials | en |
dc.relation.uri | http://dx.doi.org/10.1002/adem.200800026 | en |
dc.subject | biomaterials | en |
dc.subject | severe plastic deformation | en |
dc.subject | titanium alloys | en |
dc.title | Nanostructured titanium for biomedical applications | en |
dc.type | article | en |
dc.identifier.location | Není ve fondu ÚK | en |
dc.identifier.doi | 10.1002/adem.200800026 | |
dc.identifier.wos | 000258967500015 | |