Hodnocení popílku pomocí vyluhovacího testu "toxicity characteristic leaching procedure"

dc.contributor.authorSeidlerová, Jana
dc.contributor.authorNováčková, Martina
dc.contributor.authorWeiss, Zdeněk
dc.date.accessioned2006-10-13T14:14:50Z
dc.date.available2006-10-13T14:14:50Z
dc.date.issued2004
dc.description.abstractLeaching of iron, manganese, zinc, vanadium and copper from fly ashes from lignite, black and brown coal in power stations with grate combustion was compared. The ashes were leached according to the regulation 338/1997 by the method described in a US EPA directive, with aqueous and reagent extracts at pH 2.9 and 4.9. The performed experiments proved that the method of preparation of aqueous extracts has no influence on the amount of a leached metal. The amounts of a metal leached by the toxicity characteristic leaching procedure (TCLP) in dependence on pH of the extraction reagent differ for the studied metals and fly ashes types.en
dc.identifier.citationChemické listy. 2004, roč. 98, č. 2, s. 108-113.en
dc.identifier.issn0009-2770
dc.identifier.issn1213-7103
dc.identifier.locationVe fondu ÚKen
dc.identifier.urihttp://hdl.handle.net/10084/57119
dc.identifier.wos000189115100009
dc.language.isocsen
dc.publisherČeská společnost chemickáen
dc.relation.ispartofseriesChemické listyen
dc.relation.urihttp://chemicke-listy.cz/docs/full/2004_02_08.pdfen
dc.subjecthodnocení popílkůen
dc.subjectTCLPen
dc.subjectvyluhovací testen
dc.titleHodnocení popílku pomocí vyluhovacího testu "toxicity characteristic leaching procedure"en
dc.title.alternativeAssessment of fly ashes by TCLP leaching testen
dc.typearticleen