dc.description.abstractThis work aims to describe the interfacial interaction at the interface between refractory material and high-manganese (XT 720) and structural (11 523) steel using a wetting test up to 1600 degrees C. The contact angles were determined through the sessile drop method, and the results were put into context through degradation testing and the characterization of the interfacial interface by Energy Dispersive X-Ray (EDX), X-Ray Diffraction (XRD) analyses, and Scanning Electron Microscopy (SEM). The lowest resistance to molten steel was observed for chamotte materials, while the highest was observed for materials based on electrofused corundum. High-manganese steel was strongly erosive to the materials tested, with the wetting angle decreasing significantly from 10 to 103 degrees with decreasing Al2O3 content (an increase of 2.4 to 59.4% corundum) in the refractories. Structural steel showed wetting angles from 103 to 127 degrees for identical refractories. These results were consistent with the average erosion depth for Mn steel (0.2-7.8 mm) and structural steel (0-2.4 mm).cs
dc.language.isoencs
dc.publisherMDPIcs
dc.relation.ispartofseriesCrystalscs
dc.relation.urihttps://doi.org/10.3390/cryst12121782cs
dc.rights© 2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.cs
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/cs
dc.subjecthigh-manganese steelcs
dc.subjectstructural steelcs
dc.subjectphase interfacecs
dc.subjectreactive wettingcs
dc.subjectcontact anglecs
dc.subjectrefractory materialcs
dc.titleWetting of refractory ceramics with high-manganese and structural steel and description of interfacial interactioncs
dc.typearticlecs
dc.identifier.doi10.3390/cryst12121782
dc.rights.accessopenAccesscs
dc.type.versionpublishedVersioncs
dc.type.statusPeer-reviewedcs
dc.description.sourceWeb of Sciencecs
dc.description.volume12cs
dc.description.issue12cs
dc.description.firstpageart. no. 1782cs
dc.identifier.wos000900609400001


Soubory tohoto záznamu

Tento záznam se objevuje v následujících kolekcích

Zobrazit minimální záznam

© 2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.
Kromě případů, kde je uvedeno jinak, licence tohoto záznamu je © 2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.