dc.contributor.author | Michalek, Karel | |
dc.contributor.author | Čamek, Libor | |
dc.contributor.author | Gryc, Karel | |
dc.contributor.author | Tkadlečková, Markéta | |
dc.contributor.author | Huczala, Tomáš | |
dc.contributor.author | Troszok, Vladimír | |
dc.date.accessioned | 2012-08-01T09:03:46Z | |
dc.date.available | 2012-08-01T09:03:46Z | |
dc.date.issued | 2012 | |
dc.identifier.citation | Materiali in Tehnologije. 2012, vol. 46, issue 3, p. 297-303. | cs |
dc.identifier.issn | 1580-2949 | |
dc.identifier.issn | 1580-3414 | |
dc.identifier.uri | http://hdl.handle.net/10084/94950 | |
dc.description.abstract | The article deals with the results of the experimental heats performed in the electric steel plant of TŘINECKÉ ŽELEZÁRNY, a.
s. (TŽ, a. s.). The aim was to verify the possibility of deep desulphurization of steel in the basic 10-t electric arc furnace.
Experimental procedures making use of the industrially produced synthetic slag were applied in the production of the high-alloy
chrome steels and the middle-alloy tool steels, where the desulphurization, in terms of thermodynamics, is a more demanding
process than the chrome-nickel steel desulphurization. With the use of the technological processes it is possible to achieve low
contents of sulphur in steel, below mass fraction 0.003 %. Achieving these contents depends on a suitable slag basicity, and, in
particular, on the ratio of CaO/Al2O3. Based on the analysis of the results, a critical factor significantly affecting the final
content of the sulphur and thus the efficiency of the desulphurization of steel, the content of FeO in the reduction slag, is
carefully considered. A higher MgO content in slag (up to w = 25 %) had no significant influence on the results of the steel
desulphurization. | cs |
dc.format.extent | 924215 bytes | cs |
dc.format.mimetype | application/pdf | cs |
dc.language.iso | en | cs |
dc.publisher | Inštitut za kovinske materiale in tehnologije | cs |
dc.relation.ispartofseries | Materiali in Tehnologije | cs |
dc.relation.uri | http://mit.imt.si/Revija/izvodi/mit123/michalek.pdf | cs |
dc.subject | steel | cs |
dc.subject | desulphurization | cs |
dc.subject | synthetic slag | cs |
dc.subject | basicity of slag | cs |
dc.title | Desulphurization of the high-alloy and middle-alloy steels under the conditions of an eaf by means of synthetic slag based on CaO-Al2O3 | cs |
dc.title.alternative | Razžvepljanje močno in srednje legiranih jekel
v elektroobločni peči s sintetično žlindro na
osnovi cao-al2o3 | cs |
dc.type | article | cs |
dc.identifier.location | Není ve fondu ÚK | cs |
dc.rights.access | openAccess | |
dc.type.version | publishedVersion | cs |
dc.type.status | Peer-reviewed | cs |
dc.description.source | Web of Science | cs |
dc.description.volume | 46 | cs |
dc.description.issue | 3 | cs |
dc.description.lastpage | 303 | cs |
dc.description.firstpage | 297 | cs |
dc.identifier.wos | 000305657100018 | |