Relationship of surface and bulk resistivity in the case of mechanically damaged fibre reinforced red ceramic waste aggregate concrete

dc.contributor.authorHorňáková, Marie
dc.contributor.authorLehner, Petr
dc.date.accessioned2021-02-10T08:41:10Z
dc.date.available2021-02-10T08:41:10Z
dc.date.issued2020
dc.description.abstractElectrical resistivity is an important physical property of concrete, directly related to the chloride-induced corrosion process. This paper analyses the surface resistivity (SR) and bulk resistivity (BR) of structural lightweight waste aggregate concrete (SLWAC). The studied concrete mixture contained waste material-red ceramics fine aggregate and artificial expanded clay coarse aggregate. Red ceramic is a frequent waste material remaining after the demolition of buildings or unsatisfactory building material production and is among the least used construction waste. Therefore, its use is desirable in terms of sustainability; in some cases, it can reliably replace the conventional aggregate in a concrete mixture. The relationship between SR and BR was determined in the case of standard specimens and mechanically damaged specimens (to 50% and 100% of ultimate strength capacity-USC). Two different instruments were utilised for the investigation-a 4-point Wenner probe meter and an RCON tester. The results of standard specimens support the theoretically derived correction ratio, but in the case of mechanically damaged specimens, the ratio is more scattered, which is related to the mechanical damage and the amount of fibre.cs
dc.description.firstpageart. no. 5501cs
dc.description.issue23cs
dc.description.sourceWeb of Sciencecs
dc.description.volume13cs
dc.identifier.citationMaterials. 2020, vol. 13, issue 23, art. no. 5501.cs
dc.identifier.doi10.3390/ma13235501
dc.identifier.issn1996-1944
dc.identifier.urihttp://hdl.handle.net/10084/142810
dc.identifier.wos000597617500001
dc.language.isoencs
dc.publisherMDPIcs
dc.relation.ispartofseriesMaterialscs
dc.relation.urihttp://doi.org/10.3390/ma13235501cs
dc.rights© 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.cs
dc.rights.accessopenAccesscs
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/cs
dc.subjectconcretecs
dc.subjectdiffusioncs
dc.subjectdurabilitycs
dc.subjectred ceramic waste aggregatecs
dc.subjectresistivitycs
dc.subjectfibrecs
dc.subjectmechanical damagecs
dc.titleRelationship of surface and bulk resistivity in the case of mechanically damaged fibre reinforced red ceramic waste aggregate concretecs
dc.typearticlecs
dc.type.statusPeer-reviewedcs
dc.type.versionpublishedVersioncs

Files

Original bundle

Now showing 1 - 1 out of 1 results
Loading...
Thumbnail Image
Name:
1996-1944-2020v13i23an5501.pdf
Size:
27.71 MB
Format:
Adobe Portable Document Format
Description:

License bundle

Now showing 1 - 1 out of 1 results
Loading...
Thumbnail Image
Name:
license.txt
Size:
718 B
Format:
Item-specific license agreed upon to submission
Description: